Cutting

Different options are available for cutting glass. The most frequent method is to score the surface with a glass cutter and to then break the glass along the scored line. This technique can be used for right-angled cuts, for curves and free forming, and for cutting laminated glass to specific customer requirements.
Scoring the glass with a glass cutter
Breaking the glass along the scored line
Preparing to break the glass along the scored line
Glass broken along the scored line according to customer specifications