CONTURAN® Tough AS: The superior choice


At a Glance
50 % higher impact resistance compared to chemically toughened standard float glass – CONTURAN® Tough AS
Benefits
- More than 50 % stronger than comparable float glass
- Reduction of reflection by more than 90 % to below 1 %
- Proven mechanical and chemical resistant anti-reflective coating
- Reduced risk of breakage, increased safety
- Weight reduction by using thinner substrate with same impact resistance
- Compatible with high resolution touch displays
- Various processing options for individual customization are available
Area of Applications
- Medical displays
- HMI industry displays
- Ruggedized displays
- Outdoor displays
- Touch-screen displays
- 4K / 8K displays




Technical Information
CONTURAN® Tough AS is based on durable aluminosilicate glass with a unique anti-reflective coating, optimized for chemical tempering, offering outstanding optical performance and high durability.
It is available as chemically toughened, customized cover glass with several processing options available, e.g. screenprinting, easy-to-clean/anti-finger print coating, laminating etc.
It is available as chemically toughened, customized cover glass with several processing options available, e.g. screenprinting, easy-to-clean/anti-finger print coating, laminating etc.