PYRANOVA® for exterior applications

At a glance
PYRANOVA® for exterior applications is a special glass for use in external or particulary difficult situations, a clear composite safety glass for fire resistant glazing that offers fire resistant properties in accordance with DIN EN ISO 12543.
Depending on its structure, it is manufactured from at least two float glass panes with transparent, fire resistant intumescent interlayers and an external pane made of laminated safety glass.
Depending on its structure, it is manufactured from at least two float glass panes with transparent, fire resistant intumescent interlayers and an external pane made of laminated safety glass.
Technical data
Product |
Fire Rating |
Thickness | Weight |
Light Transmission |
Ug-Value |
Sound Reduction |
---|---|---|---|---|---|---|
acc. EN 13501-2 |
[mm]
|
[kg/m2]
|
[%]
|
[W/m2K]
|
[dB]
|
|
Exterior | ||||||
PYRANOVA® EW | EI 15 / EW 30 |
10
|
24
|
87
|
5.4
|
36
|
PYRANOVA® EW | EI 15 / EW 30 |
14
|
32
|
86
|
5.2
|
38
|
PYRANOVA® 30 | EI 30 |
19
|
44
|
83
|
5
|
38
|
PYRANOVA® 45 | EI 45 / EW 60 |
19
|
44
|
85
|
5
|
38
|
PYRANOVA® 60 | EI 60 |
27
|
61
|
86
|
4.7
|
41
|
PYRANOVA® 90 | EI 90 |
40
|
93
|
83
|
4.1
|
44
|
PYRANOVA® 120 | EI 120 |
54
|
116
|
74
|
2.5
|
44
|