Broadband AR

Description
Anti-reflection coating in accordance with ISO 9211.Our broad band AR coatings can be applied to a wide range of different glasses in order to minimize the Fresnel reflections of the substrate.
This coating can be optimized for your requirements in the range of 350 nm to 1000 nm.
Features
- The maximum diameter of the substrate is 350 nm.
- The coating is washable and scratch resistant.
- The operating temperature is up to 250 °C for several hours.
- Reflection r over a large range of wavelengths.
Additional functions
On special request we can add the following functions to the AR coating:- Abrasion resistance
- Humidity resistance
- Resistance against acids or alkalines
- Easy cleaning
Detailed specifications on request.