MICROCROWN Microscopy Glass

empty

Exceptional clarity 

MICROCROWN up-drawn soda-lime glass has one of the lowest iron contents in the market today.

It has high luminous transmittance and an excellent colorless appearance. MICROCROWN is available as sheet glass in a thickness of 1.0 mm.

Its unique composition makes MICROCROWN an excellent glass for microscope slides where low auto-fluorescence and chemical resistance are required.