NIR cut filter

Description
Coated filter glass (volume filter) with an anti-reflection layer according to ISO 9211. This combination of an absorption filter glass and interference filter coatings ideally combines the two filter technologies.Features
- The right glass for any application can be chosen from a large portfolio of different volume filters. Filters can thus be produced in different thicknesses.
- The maximum diameter of the substrate is 200 nm.
- The coating is particularly dense and resistant. It permanently protects glass from moisture corrosion.
Additional functions
On special request we can add the following functions to the filter:- Extended protection against abrasion.
Detailed specifications on request.