The distinctive quality feature of halogen lamps for the automotive industry is first and foremost the long-life cycle. Special glass tubing made from aluminosiliate glass are predestined for use in H4 and H7 lamps in view of their high temperature resistance and thermal endurance. At the same time, processing these glass types which are alkali-free and whose expansion coefficient is matched to the molybdenum filament is straightforward.

Today, SCHOTT ranks as one of the worldwide leading suppliers of special glass tubing for the production of automotive halogen lamps.