Large Scale Feedthroughs

Safety for extreme requirements:

In chemical plants and pressure vessel construction, safety is the top priority, especially when encountering critical media. Our compression-glass cable feed-throughs for pressure vessels and chemical plants cope perfectly with such demands.



  • Heat resistant: -200 to + 240 °C
  • Pressure resistant: High vacuum up to over 500 bar
  • Gastight: < 1x10 -6 mbar -1 helium
  • Non-aging (made of glass and metal)
  • Corrosion resistant: also available in stainless steel


Thanks to these excellent characteristics and our many years of manufacturing experience, SCHOTT's hermetically sealed, large-scale feed-throughs are the really safe solution.

Please contact us for more information!

Contact: Nicola Leatham
Phone: 01785 223166
Fax: 01785 223522
Email: info.uk@schott.com

Contact

SCHOTT UK Ltd

Sales Office
Drummond Road
Astonfields Industrial Estate
ST16 3EL Stafford
United Kingdom
 +44 (0)1785 223166
 +44 (0)1785 223522
E-mail
More contacts