CONTURAX® Pro - Precision Drawn Profile Tubing

CONTURAX® Pro - profile glass tubing
CONTURAX® Pro - profile glass tubing: individual angles and high surface planarity.

As an expert in the field of special glass, SCHOTT has succeeded in using its years of experience to develop a new type of non-round glass tubing: CONTURAX® Pro. Made from high-quality DURAN® borosilicate glass, this profile tubing with three or more angles is manufactured by a new, patented, continuous direct drawing process. This makes it possible to produce large quantities with uniform high quality and at an attractive price.

Product benefits and properties at a glance
  • High planarity and surface quality.
  • Geometric accuracy for precise working.
  • Direct manufacture in a continuous, patented drawing process.
  • Wide spectrum of shapes and dimensions, with the possibility of realizing customer-specified angles and asymmetrical forms.
  • Wide variety of surface finishes from smooth to profiled*
CONTURAX® Pro profile tubing also offers high transparency and thermal shock resistance, hard/smooth surfaces for the greatest resistance to scratches and tolerance of conventional cleaning agents.

Product

Inquiry



Contact

SCHOTT-Rohrglas GmbH

Erich-Schott-Strasse 14
95666 Mitterteich
Germany
 +49 (0)9633/80-0
 +49 (0)9633/80-614
E-mail
Directions
More contacts
Science Forum

User name

Password

Remember me

Forgot password?

Register