Range available

Thickness 3.75 mm / ~0.15 in.
Tolerance on thickness ± 0.25 mm / ±1 mil
Dimensions on request
Dimensional tolerance ± 1 mm / ±0.04 in.
Form supplied Flat, fire polished
thermally tempered


Other forms of supply are available on request.

As UVILEX™ 390 Z is subject to a considerable amount of heat, the glass is manufactured exclusively in a thermally tempered version.

Mechanical properties

Density 2.56 g/cm³
Maximum service temperature 260°C
Bending strength increase > 100 N/mm²
Thermal shock resistance TWB 180°C
Resistance to temperature gradient over pane surface 150 K


The above data for UVILEX™ 390 Z is valid for this glass in the thermally tempered state, undrilled and without cut-outs.

Light source
Multiplication factors compared to daylight
Increase in length of exposure with UVILEX™ 390 Z
without UV-Filter
with UVILEX™ 390 Z
Tungsten halogen and fluorescent lamps
2
4
100 %
Metal halide lamps (HQI-TS)
1.5
2.5
66 %


Multiplication factors for various lamps compared to daylight 1)


1) Source: Osram technical information 08/84

Contact

Architecture + Design
SCHOTT AG

Hattenbergstraße 10
55122 Mainz
Germany
 +49 (0)5187/771-574
 +49 (0)3641/2847-437
E-mail
Directions
More contacts
Trade Fairs & Events

04.07 - 05.07.2012

Sicherheitsexpo

Munich

More trade fairs