D 263® T eco

Applications





D 263® T eco glass



Thin glass type D 263® T eco is a colorless borosilicate glass which is produced without refining agents arsenic and antimony, using the down-draw technology process, which enables production in a very thin thicknesses between 0.03 and 1.1 mm.



This glass type is suitable for applications where the following properties are required:

  • Production without refining agents arsenic and antimony

  • Low-level mobility of alkali ions

  • Coefficient of thermal expansion close to ceramic

  • High chemical resistance

  • High transmission

  • Smooth fire-polished surface

D 263® T eco is available in many different thicknesses as stock sheets as well as in custom shapes such as squares or round wafers.

Thin Glass D 263® T eco - Product Flyer
Contact

Advanced Optics
SCHOTT AG

Hattenbergstrasse 10
55122 Mainz
Germany
 +49 (0)6131/66-1812
 +49 (0)3641/2888-9047
E-mail
Directions
More contacts
Trade Fairs & Events

04.07 - 05.07.2012

Sicherheitsexpo

Munich

More trade fairs