SCHOTT Home
Language english deutsch

Glass processing

Competence in producing
and processing glass

High precision
cutting

Shaping glass

Complete range of
glass processing

Applications

Technical possibilities



Competence in producing and processing glass

An almost infinite variety of shapes and compositions can be achieved today with glass. SCHOTT processes a wide range of different types of glass in thicknesses of 0.5 mm to 19 mm. The various types of glass can be processed and refined using a wide variety of techniques, such as grinding, polishing, drilling, sandblasting, molding and toughening. This allows for even the most challenging customer demands to be met.


B 270®
High transparency, low iron glass for technical applications. High transmittance, even with greater thicknesses. Also available as profile rod.

KG1 glass
Cold light or thermal protection glass with radiation absorption in the infrared range.

OPALIKA®
White flashed opal glass. Machine drawn two layer glass with almost ideal light diffusion in visible range of the spectrum.

Float glass
Glass manufactured using the float process. Available in various colors.



Mirrored glass
Mirrored glass with chrome coating.

UVILEX® 390 Z
UV-barrier filter glass that reduces ultraviolet radiation from artificial light sources.

BOROFLOAT®
Glass with high chemical resistance, low thermal expansion and high temperature resistance.

CONTURAN®
Optical interference anti-reflective glass, dip-coated on both sides, with various transmittances. Eliminates most irritating reflections.



Coloured glass
Machine drawn coloured glass with smooth (IMERA) and structured (ARTISTA®) surfaces in a wide range of colours.

B 270®
Highly transparent, low iron glass. Cylindrical in form with silkscreen printing or inside laser structure for use in technical lighting applications.

Filter glass
Blue-violet tinted filter glasses with variously specified UV transmittance and high absorption in the visible and infrared range, as well as clear filters with graded UV transmittances. All filter glasses feature treated edges and are thermally toughened.



Contact

Advanced Optics
SCHOTT AG

Hattenbergstrasse 10
55122 Mainz
Germany
 +49 (0)6131/66-1812
 +49 (0)3641/2888-9047
E-mail
Directions
More contacts
Trade Fairs & Events

04.07 - 05.07.2012

Sicherheitsexpo

Munich

More trade fairs