Technical Data

Stock dimensions: 406 x 258 mm
840 mm x 800 – 920 mm
1680 mm x 800 – 920 mm
other formats upon request
Available thicknesses: 0.8 mm to 10.0 mm;
< 0.8 mm and > 10.0 mm
on request
Processing: pre-cut formats
edge processing
Transmittance: > 91% in the visible wavelength range
Coefficient of expansion α (20°C; 300°C) in 10 -6 K–1 9.4
Transformation temperature Tg: 533 °C (991 °F)
Dielectric constant εr at 1MHz: 7.0
Refraction index nd: 1.523
Density ρ in g/cm3: 2.55