CONTURAN®

CONTURAN® is an anti-reflective glass with an optical interference coating on either one or both sides. SCHOTT developed a coating design that prevents optical reflections that result at the glass air passage. CONTURAN® enables almost invisible protection for many applications with the same highest light transmission and a high color rendering index combined with long durability and suitability for daily use.
The dimensions given are usually net dimensions without dipping edge. The gross dimension is supplied including the dipping edge.
Advantages:
- Reduction of irritating reflections below 1%
- High transmission (>98%) and increased contrast
- High abrasion resistance and chemical stability extends its lifetime, makes it hardly vulnerable and easy to clean
- Appears to be invisible and neutral in color, yet enables perfect viewing
- Can be adapted by applying UV or IR protection and DARO easy-to-clean / anti-fingerprint coating