8350 SCHOTT AR-Glas Soda-lime glass with a high alkali and alkaline earth oxide content
SCHOTT BORO-8330 Chemically and thermally highly resistant borosilicate glass tubing for pharmaceutical containers of the 1st hydrolytic class
SCHOTT CONTURAX Borosilicate glass tubing and rod, available in varying types of inner and outer profile
SCHOTT DURAN Borosilicate glass acc. to ISO 3585, all-purpose glass for apparatus for the chemical industry, for pipelines and laboratory
SCHOTT DURATAN Thermally prestressed (tempered) DURAN¨. Thermal prestressing noticeably improves the shock resistance of the glass.
SCHOTT DUROBAX Clear and amber, chemically highly resistant special glass tubing
SCHOTT FIOLAX 8414 Amber, neutral glass, chemically highly resistant, for pharmaceutical packaging
8412 SCHOTT FIOLAX Clear, neutral glass, chemically highly resistant, for pharmaceutical packaging
8415 SCHOTT ILLAX Chemically highly resistant special glass tubing of the 2nd hydrolytic class
1730 SCHOTT NEO1730 Alkaline earth Neodymium containing, violet colour aluminosilicate glass for high temperature applications in electrical engineering, for sealing to molybdenum, free from alkali
8095 SCHOTT 8095 Lead glass (28% PbO), electrically highly insulating, for general electro-technical applications
8100 SCHOTT 8100 Lead glass (33.5% PbO), electrically highly insulating highly X-ray-absorbing
8242 SCHOTT 8242 Borosilicate glass for sealing to Kovar metal and molybdenum, electrically highly insulating, used for production of clad tube for optical fibres and glass-to-metal seals
SCHOTT 8100 Lead glass (33.5% PbO), electrically highly insulating highly X-ray-absorbing
SCHOTT 8242 Borosilicate glass for sealing to Kovar metal and molybdenum, electrically highly insulating, used for production of clad tube for optical fibres and glass-to-metal seals
SCHOTT 8245 Borosilicate glass for sealing to Kovar metal and molybdenum with minimum x-ray absorption, chemically highly resistant
SCHOTT 8250 Electrically highly insulating and low-melting borosilicate glass for sealing to Kovar metal and molybdenum
SCHOTT 8252 Alkaline earth aluminosilicate glass for high temperature applications, for sealing to molybdenum
SCHOTT 8253 Alkaline earth aluminosilicate glass for high temperature applications, for sealing to molybdenum
SCHOTT 8270 Borosilicate glass for sealing to Kovar and molybdenum, electrically high insulating, defined UV absorption, stabilised against solarisation
SCHOTT 8271 Borosilicate glass for sealing to Kovar glass types, highly UV-blocked, stabilised against solarisation.
SCHOTT 8271N Borosilicate glass, highly UV-blocked, stabilised against solarisation, sealing to KOVAR metal
SCHOTT 8326 SBW glass, neutral glass tubing, chemically highly resistant
SCHOTT 8337B Borosilicate glass for sealing to Kovar metal and tungsten, highly UV-transmitting
SCHOTT 8347 Colourless, highly UV transmitting Borosilicate glass
SCHOTT 8360 Soft glass, lead-free
SCHOTT 8405 Highly UV-transmitting soft glass
SCHOTT 8436 Glass, particularly resistant to sodium vapours and alkaline solutions, suitable for sealing to sapphire
SCHOTT 8447 Intermediate sealing glass. Sealing with FIOLAX¨ -clear, glass 8245, glass 8250, glass 8449 and Kovar
SCHOTT 8448 Intermediate sealing glass. Sealing with DURAN¨ , glass 8449, glass 8487 and Tungsten
SCHOTT 8449 Intermediate sealing glass. Sealing with FIOLAX¨ -clear, glass 8447 and glass 8487
SCHOTT 8487 Sealing glass for Tungsten
SCHOTT 8516 IR-absorbing sealing glass for Fe-Ni, lead-free, low-evaporating
SCHOTT 8531 Soft glass, sodium-free, high lead content, for encapsulation of semiconductor components at low temperature (diodes)
SCHOTT 8532 Soft glass, sodium-free, highly lead-containing, for encapsulation of semiconductor components at low temperature (diodes)
SCHOTT 8625 IR-absorbing biocompatible glass for (implantable) transponder
SCHOTT 8650 Alkali-free sealing glass for molybdenum, especially for implosion diodes, highly lead-containing, passivation glassy
SCHOTT 8651 Tungsten sealing glass for power and PIN diodes, passivation glass
SCHOTT 8652 Tungsten sealing glass for power and PIN diodes, low melting passivation glass
SCHOTT 8687 Borosilicate glass for sealing to Tungsten, defined UV absorption, stabilised against solarisation
SCHOTT 8688 8689 Borosilicate glass, highly UV-blocked, stabilised against solarisation, sealing glass to Tungsten