ROBAX® COLOR HT

Extreme debitable

ROBAX COLOR HT is a dark, body-tinted, transparent glass ceramic which is black in appearance. Its thermal properties are the same as those of ROBAX (extremely low thermal expansion and resistance to thermal shocks as well as very high resistance to temperature/time load.) The special combination of absorption of visible light and the high transmission in the near infrared range enables the transmission of the heat radiants without blinding the onlookers.
ROBAX COLOR HT is well suited for the use in high power radiators.
Comparison ROBAX®COLOR HT and ROBAX®, in each case 4 mm
Comparison ROBAX®COLOR HT and ROBAX®, in each case 4 mm
This graph is based on individual measuring. Therefore, it can come in production-conditioned deviations

Detail view
Fuar & Organizasyonlar
21.
February
Trade fair Progetto Fuoco, Verona, Italia, 21.02 - 25.02.2018
SCHOTT, kullanıcı deneyimini zenginleştirmek ve mümkün olan en iyi hizmeti sunmak için bu Web sitesinde Çerez kullanır. Web sitesine gözatmaya devam ederek Çerez kullanmamıza onay vermiş olursunuz.