Forschungsberichte 1999-2001
Zusammensetzung, Eigenschaften und Anwendung von Spezialgläsern und Glaskeramiken
|
Bange, K.; Rauch, F.:
Surface hydration of glasses and compositional changes
The Glass Researcher 9. 1999/2000 (1), S. 4, 17
|
Brinkmann, M.; Korb, T.; Siedow, N.; Fotheringham, U.:
Fundamentals of pyrometric measurements in hot glass
6. International Conference "Advances in Fusion and Processing of Glass", Ulm (Germany), 2000 / Schaeffer, H.A., Varner, J.A., eds., Frankfurt/M.: Verl. d. Deutschen Glastechnischen Gesellschaft, 2000, S. 225-231. - (Glass Science and Technology - Glastechnische Berichte 73 C2. 2000 (Sonderbd.))
|
Conzone, S.D.; Davis, M.J.:
Low temperature joining of ZERODUR® and SiO2 for optical device manufacture
Inorganic Optical Materials III / Marker, A.J.; Davis, M.J., eds., Bellingham, WA: SPIE, 2001, S. 107-114. - (Proceedings of the SPIE ; 4452)
|
Conzone, S.D.; Hayden, J.S.; Funk, D.S.; Roshko, A.; Veasey, D.L.:
Hybrid glass substrates for waveguide device manufacture
Optics Letters 26. 2001 (8), S. 509-511
|
Conzone, S.D.; Hemrick, J.G.; Day, D.E.:
Glass formation and chemical durability of dysprosium lithium borate glasses intended for in vivo radiation synovectomy
Glass Science and Technology - Glastechnische Berichte 74. 2001 (2), S. 39-45
|
Crichton, S.N.; Tomozawa, M.; Hayden, J.S.; Suratwala, T.I.; Campbell, J.H.:
Subcritical crack growth in a phosphate laser glass
Journal of the American Ceramic Society 82. 1999 (11), S. 3097-3104
|
Davis, M.J.:
Effect of the growth treatment on two-stage nucleation experiments: the "flushing" effect
International Symposium on Crystallization in Glasses and Liquids, July, 9-12, 2000, Vaduz / Principality of Liechtenstein / ed. by W. Höland, M. Schweiger, V. Rheinberger, Frankfurt/M.: Verl. d. Deutschen Glastechnischen Gesellschaft, 2000, S. 170-177. – (Glass Science and Technology - Glastechnische Berichte 73 C1. 2000 (Sonderbd.))
|
Davis, M.J.; Marker, A.J.; Aschke, L.; Schubert, F.; Mörsen, E.; Kohlmann, H.; Mitra, I.; Alkemper, J.; Müller, R.; Taylor, J.S.; Blädel, K.L.; Hector, S.D.:
Thermal expansion and internal quality of a proposed EUVL mask substrate material: ZERODUR®(R)
Inorganic Optical Materials III / Marker, A.J.; Davis, M.J., eds., Bellingham, WA: SPIE, 2001, S. 100-106. - (Proceedings of the SPIE ; 4452)
|
Ehrmann, P.R.; Campbell, J.H.; Suratwala, T.I.; Hayden, J.S.; Krashkevich, D.; Takeuchi, K.:
Optical loss and Nd3+ non-radiative relaxation by Cu, Fe and several rare earth impurities in phosphate laser glasses
Journal of Non-Crystalline Solids 263-264. 2000, S. 251-262
|
Engel, A.; Knapp, K.; Aschke, L.; Mörsen, E.; Triebel, W.; Chojetzki, C.; Brückner, S.:
Development and investigation of high quality CaF2 used for 157 nm lithography
Lithographie for Semiconductor Manufacturing II / Mack, C.A.; Stevenson, T., eds., Bellingham, WA: SPIE, 2001, S. 298-304. - (Proceedings of the SPIE ; 4404)
|
Fankhänel, B.; Müller, E.; Mosler, U.; Siegel, W.; Beier, W.:
Electrical properties and damage monitoring of SiC-fibre-reinforced glasses
Composites Science and Technology 61. 2001, S. 825-830
|
Fotheringham, U.:
Heat transfer and temperature field determination in hot glass: contributions from Schott Proceedings of the International Scientific Colloquium on the Occasion of Otto Schott's 150th Birthday : Glass Science and Technology on the Threshold of the 3rd Millennium, December 18, 2001 / ed. by W. Pannhorst, Frankfurt/M.: Verl. d. Deutschen Glastechnischen Gesellschaft, 2001, S. 167-203. - (Glass Science and Technology - Glastechnische Berichte 74 C. 2001 (Sonderbd.))
|
Gabel, F.; Kiefer, W.; Müller, G.; Pannhorst, W.; Sprengard, R.:
On the Raman spectrum of ZrTiO4
International Symposium on Crystallization in Glasses and Liquids, July, 9-12, 2000, Vaduz / Principality of Liechtenstein / ed. by W. Höland, M. Schweiger, V. Rheinberger, Frankfurt/M.: Verl. d. Deutschen Glastechnischen Gesellschaft, 2000, S. 337. – (Glass Science and Technology - Glastechnische Berichte 73 C1. 2000 (Sonderbd.))
|
Hartmann, P.; Morian, H.F.; Jedamzik, R.:
Optical glasses and glass ceramics for large lenses and prisms
Large Lenses and Prisms / Bingham, R.G., Walker, D.D., eds., Bellingham, WA: SPIE, 2002, S. 6-20. - (Proceedings of the SPIE ; 4411)
|
Hayden, J.S.:
In search of high-power optics
Photonics Spectra 35. 2001 (9), S. 128-130
|
Marker, A.J.; Wang, B.L.; Klimek, R.:
Effect of residual stress in optical glass on the transmitted wavefront
Inorganic Optical Materials II / Marker, A.J.; Arthurs, E.G., eds., Bellingham, WA: SPIE, 2000, S. 211-218. - (Proceedings of the SPIE ; 4102)
|
Müller, M.; Rüssel, C.; Claußen, O.:
UV-VIS spectroscopic investigations of amber glass at high temperatures
Glass Science and Technology - Glastechnische Berichte 72. 1999 (11), S. 362-366
|
Pannhorst, W.:
Development and application of glass ceramics
International Symposium on Crystallization in Glasses and Liquids, July, 9-12, 2000, Vaduz / Principality of Liechtenstein / ed. by W. Höland, M. Schweiger, V. Rheinberger, Frankfurt/M.: Verl. d. Deutschen Glastechnischen Gesellschaft, 2000, S. 28-35. – (Glass Science and Technology - Glastechnische Berichte 73 C1. 2000 (Sonderbd.))
|
Pannhorst, W.:
Recent advances in glass ceramics
19. International Congress on Glass, Edinburgh, July 1-6, 2001, proceedings / Society of Glass Technology, Sheffield: Society of Glass Technology, 2001, S. 142-146
|
Peters, P.M.; Funk, D.S.; Peskin, A.P.; Veasey, D.L.; Sanford, N.A.; Houde-Walter, S.N.; Hayden, J.S.:
Ion-exchanged waveguide lasers in Er3+/Yb3+ codoped silicate glass
Applied Optics 38. 1999 (33), S. 6879-6886
|
Reinicke, R.; Friedrich, K.; Beier, W.; Liebald, R.:
SiC- and C-fiber reinforced glass matrix composites for tribological applications
Advanced Engineering Materials 3. 2001 (6), S. 423-426
|
Reinicke, R.; Friedrich, K.; Beier, W.; Liebald, R.:
Tribological properties of SiC and C-fiber reinforced glass matrix composites
Wear 225-229. 1999, S. 1315-1321
|
Reinicke, R.; Friedrich, K.; Beier, W.; Liebald, R.:
Tribologisches Verhalten von Glas-Matrix-Kompositen mit Siliziumkarbid- und Kohlenstofffasern
Materialwissenschaft und Werkstofftechnik 31. 2000 (8), S. 696-699
|
Schuster, K.; Kobelke, J.; Schwuchow, A.; Kirchhof, J.; Sprengard, R.; Peuchert, U.:
Composition and rare earth concentration effects on tellurite glasses and fibres for amplifier applications
19. International Congress on Glass, Edinburgh, July 1-6, 2001, proceedings / Society of Glass
Technology, Sheffield: Society of Glass Technology, 2001, S. 887-888
|
Sprengard, R.; Binder, K.; Brändle, M.; Fotheringham, U.; Sauer, J.; Pannhorst, W.:
On the interpretation of the experimental Raman spectrum of ß-eucryptite LiAlSiO4 from atomistic computer modeling
Journal of Non-Crystalline Solids 274. 2000, S. 264-270
|
Veasey, D.L.; Funk, D.S.; Peters, P.M.; Sanford, N.A.; Obarski, G.E.; Fontaine, N.; Young, M.; Peskin, A.P.; Liu, W.C., Houde-Walter, S.N.; Hayden, J.S.:
Yb/Er-codoped and Yb-doped waveguide lasers in phosphate glass
Journal of Non-Crystalline Solids 263-264. 2000, S. 369-381
|
Veasey, D.L.; Funk, D.S.; Sanford, N.A.; Hayden, J.S.:
Arrays of distributed-Bragg-reflector waveguide lasers at 1536 nm in Yb/Er codoped phosphate glass
Applied Physics Letters 74. 1999 (6), S. 789-791
|
Veasey, D.L.; Funk, D.S.; Sanford, N.A.; Hayden, J.S.; Bendett, M.:
Laser arrays may provide DWDM measurement tool
Laser Focus World 35. 1999 (5), S. 203-210
|
Völker, K.; Zum Gahr, K.-H.; Pannhorst, W.; Beier, W.:
Untersuchungen zur Haftreibung zwischen faserverstärktem Borosilicatglas und Kalk-Natron-Glas bei erhöhten Temperaturen
Materialwissenschaft und Werkstofftechnik 30. 1999 (1), S. 5-13
|
Völker, K.; Zum Gahr, K.-H.; Rombach, M.; Sommer, E.; Beier, W.; Pannhorst, W.:
Optimierung tribologischer und mechanischer Eigenschaften von faserverstärkten Gläsern und Glaskeramiken
Keramikverbund Karlsruhe - Stuttgart (KKS) des Landes Baden-Württemberg, 01.01.1996 - 31.12.1998: Forschungsergebnisse / F. Aldinger, D. Munz, Köln: Deutsche Keramische Gesellschaft, Wiesbaden (u.a.): Bauverl. 2000, S. 171-182. - (Fortschrittsberichte der Deutschen Keramischen Gesellschaft 15. 2000 (1))
|
Völkl, R.; Freund, D.; Fischer, B.; Gohlke, D.:
Comparison of the creep and fracture behavior of non-hardened and oxide dispersion hardened platinum base alloys at temperatures between 1200 °C and 1700 °C
Key Engineering Materials 171-174. 2000, S. 77-83
|
|
|