SCHOTT TopPac® syringes have excellent barrier properties.
Nest of Syringes
Packaging in nest and tub fits common pharmaceutical filling line requirements.
SCHOTT TopPac® prefillable polymer syringes

SCHOTT TopPac® syringes are made of COC (cyclic olefin copolymer). The ready-to-fill syringes are break resistant, light weight, and transparent with a glass-like appearance. SCHOTT has more than 10 years of experience with COC material for pharmaceutical applications. SCHOTT TopPac® syringes are available from 1 ml to 50 ml.

SCHOTT TopPac® Syringes show excellent barrier properties, no ion or heavy metal release, and a lower particle level than glass. The high moisture barrier enables the long-term storage of drugs – even in small containers. Terminal sterilization (autoclaving) after filling is possible.

The integrated luer lock of SCHOTT TopPac® syringes offers superior robustness and ease of application for the final user. High design flexibility allows customized solutions. Components for a complete set are available according to customer requirements.

SCHOTT TopPac® syringes are packed in nests and tubs, like glass syringes. They can be processed on all common syringe filling lines.

The prefillable polymer syringes comply with international quality standards such as USP, EP and JP

Syringes
SCHOTT TopPac® syringes can be delivered as complete sets, according to customer requirements.
components COC syringe
The integrated luer lock offers superior robustness (ISO 594).
Closure systems
  • Luer lock with tip cap
  • Cut flange


Accessories
The syringes can be delivered as complete sets, including plunger and plunger rod.
  • Plunger
  • Plunger rod

Packaging

All SCHOTT TopPac® syringes are delivered in nest and tub configuration, ready for the filling process.

Syringes
SCHOTT TopPac® is the packaging of choice for many pharmaceutical applications.


Applications


COC syringes are ideal for packaging and administrating a broad range of pharmaceutical compounds, such as:
  • Biotech/biopharmaceutical drugs
  • Highly viscous products like hyaluronic acid
  • Diluents like water for injection (WFI)
  • Contrast Media
  • Toxic products
  • Wide pH range products
  • Vaccines
  • Veterinary drugs


Clean room
SCHOTT TopPac® syringes are produced on state-of-the-art manufacturing equipment with advanced in-line inspection systems.
Fully integrated clean room production

The production of SCHOTT TopPac® syringes is a continuous, fully integrated process taking place in a class B clean room. It starts by transferring TOPAS® granulate from silos directly to the injection moulding machines.

Automated assembly technology is supported by in-line process control. Advanced visual inspection technology controls dimensional and cosmetic aspects. Reliable quality systems and rigid quality controls guarantee the consistent high quality of the syringe sets.

Clean room
The SCHOTT TopPac® production in class B clean room is a completely integrated process


Contact

Pharmaceutical Systems
SCHOTT AG

Hattenbergstrasse 10
55122 Mainz
Germany
 +49 (0)6131/66-1589
 +49 (0)6131/66-1916
E-mail
Directions
More contacts
Trade Fairs & Events

29.05 - 31.05.2012

FCE Pharma

Sao Paulo

04.06 - 05.06.2012

PDA FDA Glass Quality Conference

Bethesda

More trade fairs