In general, sunglass lenses are used to protect the human eye against excessive solar radiation, to reduce eye strain and to increase the visual comfort.

In order to secure fatigue-free vision, even for prolongated usage, the choice of filter depends on the ambient light level and the individual sensitivity to glare.

The European standards DIN EN 1836 + DIN EN 172 specifies the properties and the recommended application of sun glare filters.

The sun glare filters for general use are classified into 5 filtering groups, and the admissible transmittances in the UV region, the visible region and the IR region are clearly specified.

SCHOTT Ophthalmic offers:
- lens blanks with UV and IR protection
- extensive range of colors
- customer specified colors and transmissions
- contrast enhancement glasses


Physical and chemical properties according to specification