SCHOTT NEXTREMA® types of material

With NEXTREMA® we offer engineers and designers a unique glass-ceramics portfolio of six material options. All six types have the following material benefits in common:
  • High temperature & thermal shock resistance
  • A non-porous, highly resistant surface
  • High chemical resistance
  • Transmission in infrared range
  • Good mechanical strength
In addition each material type has its specific material benefits that will help designers and engineers alike realize new applications, functionalities, and designs. Explore the specific material benefits and exemplary application fields by clicking on the material types.
SCHOTT NEXTREMA® tinted glass-ceramic
SCHOTT NEXTREMA®
tinted
(712-3)
SCHOTT NEXTREMA® tinted glass-ceramic

SCHOTT NEXTREMA® tinted (712-3)


Key properties
  • Visible light reduction in combination with high infrared transmission
  • High transmission in IR-A & IR-B range
  • Highest bending strength of all NEXTREMA® types (168 MPa for 4 mm thick material)
  • Excellent thermal shock resistance of up to 800 °C


Exemplary application fields
  • Attractive cover panel for outdoor & indoor radiant heaters
  • Glare reducing cover panel for infrared heaters (e.g. paint drying)
  • Decorative element in architecture, furniture & appliance applications
SCHOTT NEXTREMA® translucent bluegrey glass-ceramic
SCHOTT NEXTREMA®
translucent bluegrey
(712-6)
SCHOTT NEXTREMA® translucent bluegrey glass-ceramic

SCHOTT NEXTREMA® translucent bluegrey (712-6)
 

Key properties
  • Visible light reduction in combination with high infrared transmission
  • High bending strength of 150 MPa (4 mm thick material)
  • Unique translucent design


Exemplary application fields
  • Stylish cover panel for outdoor & indoor radiant heaters
  • Decorative element in architecture, furniture & appliance applications
SCHOTT NEXTREM® opaque grey glass-ceramic
SCHOTT NEXTREMA®
opaque grey
(712-8)
SCHOTT NEXTREM® opaque grey glass-ceramic

SCHOTT NEXTREMA® opaque grey (712-8)
 

Key properties
  • Completely visible light blocking
  • Highest thermal insulation properties of all NEXTREMA® types due to lowest overall transmission in IR range of all
  • Very high temperature resistance of up to 950 °C


Exemplary application fields
  • Inner lining in high temperature clean room furnaces (e.g. display industry)
  • Easy-to-clean cover plate for magnetrons in high power microwave ovens
  • Decorative cover plate for zero-light radiant heaters
SCHOTT NEXTREMA® transparent glass-ceramic
SCHOTT NEXTREMA®
transparent
(724-3)
SCHOTT NEXTREMA® transparent glass-ceramic

SCHOTT NEXTREMA® transparent (724-3)

Key properties

  • Near zero thermal expansion
  • High transmission in short wave infrared range
  • Highest thermal shock resistance of all NEXTREMA® types (up to 820 °C)


Exemplary application fields
  • Cover panel for radiant heating elements in industrial processes
  • Sight window in high temperature processes
  • Carrier plate in high temperature processes
  • Substrate for transparent thin-film heating elements
SCHOTT NEXTREMA® translucent white glass-ceramic
SCHOTT NEXTREMA®
translucent white
(724-5)
SCHOTT NEXTREMA® translucent white glass-ceramic

SCHOTT NEXTREMA® translucent white (724-5)

Key properties

  • Visible light reduction in combination with high infrared transmission
  • Broadest overall IR transmission window of all NEXTREMA® types
  • Excellent chemical resistance & surface hardness
  • Transparent for LED light sources


Exemplary application fields
  • Glare reducing radiant heater cover in industrial processes
  • Stylish cover panel for outdoor & indoor radiant heaters
  • Hotbed for 3D printers
SCHOTT NEXTREM® opaque white glass-ceramic
SCHOTT NEXTREMA®
opaque white
(724-8)
SCHOTT NEXTREM® opaque white glass-ceramic

SCHOTT NEXTREMA® opaque white (724-8)

Key properties

  • Highest maximum temperature resistance of up to 950°C of all NEXTREMA® types
  • Unique visible light diffusing properties
  • High thermal insulation due to low transmission in short wave IR range
  • Highest chemical resistance of all NEXTREMA® types


Exemplary application fields
  • Inner lining in high temperature clean room furnaces
  • Easy-to-clean cover plate for magnetrons in high power microwave ovens
  • Decorative element in architecture, furniture & appliance applications