Optical properties

Six transmission profiles in visible & infrared range
 
NEXTREMA® offers six unique transmission profiles in visible and infrared range. The resulting functionalities combined with the glossy appearance of NEXTREMA® will inspire designers and engineers to develop revolutionary applications and designs. 


 
Key properties
     Benefits
   
6 transmission profiles in
visible and infrared range
  • Various design options and effects on visible light (transparent, diffusing, blocking)
  • Transparency for LEDs (except 712-8)
  • IR-A & IR-B filter function (724-8 & 712-8)
  • Good thermal insulation properties due to low transmission for IR radiation (712-8 & 724-8)
High transmission for infrared radiation from 800nm – 4500 nm
  • Excellent transparency for infrared heat, especially for 2 mm & 3 mm material thicknesses
  • Good match with IR heating elements

Transmission

The transmission values are measured for a polished sample of a specific thickness.
This graph is based on data from individual measurements. Deviations may result from manufacturing process.
Typical transmission graph of different ceramization states with sample thickness of approximately 4 mm.
Transmission curve
SCHOTT NEXTREMA® tinted (712-3)
Transmission curve
SCHOTT NEXTREMA® transparent (724-3)
Transmission curve
SCHOTT NEXTREMA® translucent bluegrey (712-6)
Transmission curve
SCHOTT NEXTREMA® translucent white (724-5)
Transmission curve
SCHOTT NEXTREMA® opaque grey (712-8)
Transmission curve
SCHOTT NEXTREMA® opaque white (724-8)
News, Trade Fairs & Events
01.
May
Trade fair Ceramics Expo, Cleveland, OH, USA, 01.05 - 03.05.2018
23.
April
Trade fair Hannover Messe Industrie, Hannover, Germany, 23.04 - 27.04.2018
SCHOTT uses Cookies on this Website to enhance the user experience and provide the best possible Service. By continuing to browse the Website, you consent to our use of Cookies.