Chemical properties

Highly resistant surface against chemical attacks
 
Only special glasses used in lab­o­ra­to­ries can compete with the re­sis­tance to acids and bases of
NEX­TREMA® glass-ce­ram­ics. The highly corrosion resistant surface ensures a reliable material performance and stable process environments even under corrosive conditions.
 

Key properties
     Benefits
   
Chemically resistant surface comparable to laboratory glassware
  • No material degradation and thus stable performance in corrosive environments
  • Reliable protection against gases, acids and bases in aggressive process environments
Non-porous, smooth surface
  • No outgassing in vacuum environments
  • No generation or adhesion of particles

Principal constituents (reference: DIN EN 1748-2-1)
The principal constituents of all the ceramic materials are as follows:

Component
 

Symbol  

Percentage per mass  
Silicon dioxide SiO2 50 % – 80 %
Aluminium oxide Al2O3 15 % – 27 %
Lithium oxide Li2O 0 % – 5 %
Zinc oxide ZnO 0 % – 5 %
Titanium oxide TiO2 0 % – 5 %
Zirconium oxide ZrO2 0 % – 5 %
Magnesium oxide MgO 0 % – 8 %
Calcium oxide CaO 0 % – 8 %
Barium oxide BaO 0 % – 8 %
Sodium oxide Na2O 0 % – 2 %
Potassium oxide K2O 0 % – 2 %
Other (trace content on request)   0 % – 5 %
The materials do not contain any harmful substances according to the European
directive 2002/95/EC “Hazardous Substances in electrical and electronically
Equipment” and fulfill the terms of RoHS without any concerns.  

 
 
Federal Republic of Germany waste disposal regulations differentiate five classes
of waste, Z0 (non-restricted disposal), Z3 (household waste), and up to Z5 (highly toxic waste). All NEXTREMA® materials are classified as non-restricted disposal. 
Local government regulations may differ. Please contact the local authority if
needed. NEXTREMA® must not be disposed of in recycling boxes for standard glass (e.g. glass bottles).

 
End of life usage
The chemical resistance of NEXTREMA® is more extensive than that of most other
comparable materials.

 
 Chemical resistance

  Tinted
(712-3)
Translucent bluegrey
(712-6)
Opaque grey
(712-8)
Transparent
(724-3)
Translucent white
(724-5)
Opaque white
(724-8)
Hydrolytic Resistance
HGB (ISO 719)
1 1 1 1 1 1
Acid Resistance
S (DIN 12116)
2 2 2 2 1 1
Alkali Resistance
A (ISO 695)
1 2 2 1 1 1
1 = High resistance / low solubility
2 = medium resistance / medium solubility
3 = low resistance / high solubility
News, Trade Fairs & Events
01.
May
Trade fair Ceramics Expo, Cleveland, OH, USA, 01.05 - 03.05.2018
23.
April
Trade fair Hannover Messe Industrie, Hannover, Germany, 23.04 - 27.04.2018
SCHOTT uses Cookies on this Website to enhance the user experience and provide the best possible Service. By continuing to browse the Website, you consent to our use of Cookies.