Epoxysilane Coating (E)

The NEXTERION® epoxysilane coating is a very commonly used surface chemistry for a broad range of diagnostic applications. These substrates have a multi-purpose epoxysilane layer that will covalently bind most types of bio-molecules including amino- and non-modified DNA, RNA, and proteins.

The defect-free surface features a uniform epoxysilane layer that provides a high covalent coupling efficiency together with a very low background. The robust and stable surface chemistry easily allows long print runs. This type of substrate is easy to use, protocols for many applications are published in literature.

Produced in ISO class 5 clean room conditions using a standardized process and running a stringent quality control system, epoxysilane coated substrates are available in standard as well as in custom formats.
  • Coating Chemistry
  • Shelf Life
    Twelve months for sealed packages at room temperature.
  • Immobilisation Method
    Covalent binding via amino-, thiol- and hydroxyl-reactive chemistry.
  • Probe Types
    • Amino-modified oligonucleotides (necessary for <20 mers)
    • Unmodified oligonucleotides
    • PCR products
    • ZIP code oligonucleotides
    • BACs, PACs, YACs, plasmids
    • L-DNA
    • cDNA
    • RNA
    • Serum samples
    • Proteins
    • Antibodies
    • Peptides
    • Glucans
Trade Fairs & Events
Trade fair Lab-on-a-Chip and Microfluidics Europe 2018, Rotterdam, Netherlands, 05.06 - 06.06.2018
Trade fair Workshop Microarrays, Zurich, Switzerland, 05.06 - 06.06.2018
Trade fair Lab-on-a-Chip and Microfluidics World Congress 2018, Coronado Island, USA, 01.10 - 03.10.2018
SCHOTT uses Cookies on this Website to enhance the user experience and provide the best possible Service. By continuing to browse the Website, you consent to our use of Cookies.