Versions supplied:

“SCHOTT Ceramat” FN with an unperforated surface for applications in industrial furnaces, drying plants, gas fires

“SCHOTT Ceramat” FP with a perforated surface for use in gas-fired heating units, water boilers, “Ceran Matic” gas cooking systems

Product properties

  • Easily permeable for gas
  • Stable combustion with all current gas types
  • Suitable for infrared radiant burners, blue flame burners and burners for yellow flames
  • Low CO and NOx emissions in wide modulation range
  • Variable geometries
  • Immediate heating up and cooling down through low thermal mass
  • Temperature resistant up to 1000°C