SCHOTT Lighting and Imaging offers high precision, coherent glass capillary arrays in linear and plate formats.
|
 |
|
 |
Linear and Plate Array Configurations Without Interstitial EMA
|
Energetic Particle Detector Systems
Liquid-Filled Fiber Systems
Focusing / Collimating Components
Neutron Channeling Components
Biotechnology Micro Pore Components
Telecommunication Alignment Components
|
Development Activities
|
Development continues in optimizing higher length-to-diameter ratios and increased cross-sectional areas within the arrays. Pore geometry and packing patterns can be customized.
|
Linear Arrays
|
Linear arrays consist of close-packed pattern with individual pore sizes ranging from 50 microns up to 1 mm. For optical applications they can be supplied with absorbing fibers (EMA) to reduce optical cross talk.
|
Shown With and Without Absorbing Fibers (EMA)
|
Plate arrays are produced by etching processes with precisely-aligned pores from 10 microns to 1 mm.
SCHOTT Lighting and Imaging, Inc. is a world leading custom designer and manufacturer of state of-the art fused, flexible and rigid fiber optic imaging components. We custom-produce a wide variety of components for medical and dental x-ray imaging, night vision, information display, industrial, medical, instrumentation and scientific applications.
|
| GLASS TYPE |
Borosilicate Glass |
Lead Silicate Glass |
| Density |
2.3g/cm3 |
3.0 g/cm3
|
| Refractive Index |
1.49 |
1.56 |
| Thermal Expansion |
50x10-7/°C |
90x10-7/°C |
| Anneal Temperature (1013) |
510°C |
435°C |
| Softening Point (107.6) |
715°C |
630°C |
|
| SPECIFICATIONS* |
Linear Format |
Plate Format |
| Capillary Pore Sizes |
50 microns to 1 mm |
10 microns to 1 mm |
| Number of Pores |
1 to 200,000 |
1 to 200,000 |
| Length (Thickness) |
Up to 2 meters |
Up to 25 mm |
| Cross Section |
Up to 25 mm |
Up to 25 mm |
| Configurations, Patterns |
Hexagonal,
Square |
Hexagonal,
Square |
| EMA (Extra Mural Absorption) |
Optional |
Optional |
| Glass Types |
Borosilicate
Lead Silicate |
Lead Silicate |
|
SCHOTT Lighting and Imaging continually upgrades its products and specification; changes are subject to change without notice. Version 1/99
For more information or product specifications relating to your application, contact SCHOTT Lighting and Imaging' Technical Sales Departments. We are committed to applying our proven capabilities to meet your custom imaging requirements.
|
|