SCHOTT Home

Capillary Arrays

COHERENT CAPILLARY ARRAYS

Linear and Plate Formats

All SCHOTT Arrays are Manufactured to Customer Specifications

Applications

SCHOTT Lighting and Imaging offers high precision, coherent glass capillary arrays in linear and plate formats.




Linear and Plate Array Configurations Without Interstitial EMA
Energetic Particle Detector Systems
Liquid-Filled Fiber Systems
Focusing / Collimating Components
Neutron Channeling Components
Biotechnology Micro Pore Components
Telecommunication Alignment Components


Development Activities

Development continues in optimizing higher length-to-diameter ratios and increased cross-sectional areas within the arrays. Pore geometry and packing patterns can be customized.

Linear Arrays

Linear arrays consist of close-packed pattern with individual pore sizes ranging from 50 microns up to 1 mm. For optical applications they can be supplied with absorbing fibers (EMA) to reduce optical cross talk.

Plate Arrays

Shown With and Without Absorbing Fibers (EMA)
Plate arrays are produced by etching processes with precisely-aligned pores from 10 microns to 1 mm.


SCHOTT Lighting and Imaging, Inc. is a world leading custom designer and manufacturer of state of-the art fused, flexible and rigid fiber optic imaging components. We custom-produce a wide variety of components for medical and dental x-ray imaging, night vision, information display, industrial, medical, instrumentation and scientific applications.

GLASS TYPE Borosilicate Glass Lead Silicate Glass
Density 2.3g/cm3 3.0 g/cm3
Refractive Index 1.49 1.56
Thermal Expansion 50x10-7/°C 90x10-7/°C
Anneal Temperature (1013) 510°C 435°C
Softening Point (107.6) 715°C 630°C


SPECIFICATIONS* Linear Format Plate Format
Capillary Pore Sizes 50 microns to 1 mm 10 microns to 1 mm
Number of Pores 1 to 200,000 1 to 200,000
Length (Thickness) Up to 2 meters Up to 25 mm
Cross Section Up to 25 mm Up to 25 mm
Configurations, Patterns Hexagonal,
Square
Hexagonal,
Square
EMA (Extra Mural Absorption) Optional Optional
Glass Types Borosilicate
Lead Silicate
Lead Silicate


SCHOTT Lighting and Imaging continually upgrades its products and specification; changes are subject to change without notice. Version 1/99

For more information or product specifications relating to your application, contact SCHOTT Lighting and Imaging' Technical Sales Departments. We are committed to applying our proven capabilities to meet your custom imaging requirements.






SCHOTT Lighting and Imaging is ISO 9001:2000, ISO 13485:2003 registered


Contact

Lighting and Imaging
SCHOTT AG

Otto-Schott-Strasse 2
55127 Mainz
Germany
 +49 (0)6131/66-7794
 +49 (0)6131/66-7850
E-mail
Directions
More contacts
Top news
More news
Trade Fairs & Events

13.03 - 15.03.2012

Medtec 2012

Stuttgart

20.03 - 22.03.2012

Vision China (Shanghai) 2012

Shanghai

27.03 - 29.03.2012

Aircraft Interiors Expo

Hamburg

More trade fairs