15.06.2009, Advanced Optics
SCHOTT AG
Large Format Synthetic Fused Silica

Homogeneous and free from inclusions: SCHOTT “Lithosil” for lenses of up to 700 mm in diameter

Jena/Munich (Germany), June 15, 2009 — At “Laser – World of Photonics”, SCHOTT will be presenting a large plate made of the synthetic fused silica “Lithosil” in a typical format of 1050 x 580 x 35 mm. This exhibit stands for the expertise that SCHOTT has in manufacturing homogeneous, ultrapure and bubble-free blanks for large format lenses.

These products are now available on a standard basis in dimensions of up to 700 mm in diameter and 110 kg respectively. Furthermore, homogeneity of up to < 5 ppm is achieved and they are completely free of all types of inclusions or bubbles. These products are known for their extremely high transmission in the UV and VIS range, as well as extremely low stress birefringence.

The sample on display that is made of the synthetic fused silica “Lithosil” rounds off the portfolio of large format blanks that SCHOTT offers. At the same time, formats of up to 1000 mm in diameter can also be achieved using traditional optical glass types, such as N-BK7, LLF1 and others. Typical applications for large “Lithosil” blanks include astronomy and lithography, but also large format lenses for use in conventional optics.

“With these large formats, our unique expertise lies in customer-specific forming of shapes,” notes Peter Maushake, Product Manager at SCHOTT Advanced Optics for the “Lithotec” products. In addition to the dimensions presented here, a wide variety of different geometries are possible thanks to customer-specific slumping. “Our colleagues who work in sales and research and development support our customers in realizing their projects. Virtually anything is possible,” Maushake points out.

SCHOTT is an international technology group that sees its core purpose as the lasting improvement of living and working conditions. To this end, the company has been developing special materials, components and systems for 125 years. The main areas of focus are the household appliances industry, pharmaceuticals, solar energy, electronics, optics and the automotive industry. The SCHOTT Group is present in close proximity to its customers with production and sales companies in all its major markets. The Group’s approximately 17,300 employees generated worldwide sales of approximately 2.2 billion Euros in the fiscal year 2007/2008. The company's technological and economic expertise is closely linked with its social and ecological responsibility. The SCHOTT AG is an affiliate of the Carl-Zeiss-Stiftung (Foundation).

Number of characters: 1775 (including empty spaces)

Advanced Optics
SCHOTT AG
 
Further information:
Advanced Optics
SCHOTT AG
Christine Fuhr
PR Manager
Corporate Public Relations
Tel. +49 (0) 6131 / 66-4550
Fax +49 (0) 6131 / 66-4041
E-mail
 
back Top




Contact

Lighting and Imaging
SCHOTT AG

Otto-Schott-Str. 2
55127 Mainz
Germany
 +49 (0)6131/66-0
 +49 (0)6131/66-7705
E-mail
More contacts
Trade Fairs & Events

27.11 - 04.12.2009

RSNA

Chicago

10.12 - 13.12.2009

Industrial Automation INDIA

Bombay Exhibition Centre
Western Express Highway
Goregaon East, Mumbai 400 063

23.03 - 25.03.2010

MEDTEC

Stuttgart

21.04 - 22.04.2010

BIOMEDevice

Boston

More trade fairs