Leached Image Bundle

Leached fiber bundles are flexible, coherent image guides used for transmitting optical images from one end to the other. Our new “Next Generation” leached fiber bundles are now available to set a new standard in the marketplace.

When combined with custom optics, these bundles can be found in endoscopes for medical, veterinary and industrial applications. For improved market responsiveness, several standard sizes are available in stock.

Custom leached fiber bundles can be manufactured upon request.
Trade Fairs & Events
15.
May
Trade fair Optatec, Frankfurt, Germany, 15.05 - 17.05.2018
30.
May
Trade fair Materials, Veldhoven, Netherlands, 30.05 - 31.05.2018
12.
June
Trade fair EPHJ-EPMT-SMT, Genève, Switzerland, 12.06 - 15.06.2018
05.
February
Trade fair SPIE Photonics West, San Francisco, CA, USA, 05.02 - 07.02.2019
Contact
SCHOTT AG
Lighting and Imaging

Otto-Schott-Strasse 2
55127 Mainz
Germany
E-Mail to SCHOTT+49 (0)6131/66-7844
SCHOTT uses Cookies on this Website to enhance the user experience and provide the best possible Service. By continuing to browse the Website, you consent to our use of Cookies.