Coatings and tinted panels

SCHOTT ROBAX® Energy Plus coatning
At a glance

The power package for your fireplace: ROBAX® Energy Plus is the first glass-ceramic fire panel with a heat reflecting coating. It is available in a flat version as well as in a rounded form for the first time. The advantage is an energy-friendly fireplace: While visible light can easily pass through the panel, some of the heat radiation is reflected back into the combustion chamber. This can result in a noticeable gain in stored energy – ROBAX® Energy Plus.



 
Product benefits
 
Up to 35 % of the heat radiation is reflected back into the combustion chamber. The result: the energy radiation passing through the panel is reduced and the temperature in the combustion chamber is significantly increased. The extra energy gained can be used for more efficient heating water conduits or as additional stored energy.

The higher temperatures in the combustion chamber generally causes better combustion and results in lower emission values.

Even when the heat runs high, ROBAX® Energy Plus is resistant to high temperatures. The temperature resistance is approximately 650 °C (1,202 °F). The efficiency of the coating is therefore maintained over time.

The coating can result in less soiling on the panel, in particular due to soot, which makes cleaning the glass-ceramic distinctly easier.

The reduced radiation means that the installation area is heated more pleasantly and evenly. Moreover, the floor temperature in front of the heating appliance remains cooler. This means that furniture can be placed closer to the visible area of the appliance, thus offering increased enjoyment of the fire experience.

The SCHOTT application technology laboratory guarantees comprehensive application servicing.

Stress temperature  
                                              
650 °C/ 1,202 °F       100 hours
600 °C/1,112 °F     1,000 hours

Technical data
 
 
Glass thickness 4 and 5 mm
Max. usable area 1,914 mm x 1,060 mm
Versions Rounded (dimensions upon request), flat,
coating is always on outer side
Temperature resistance   up to 650 °C (1,202 °F)
Effect of the coating Additional stored energy, improved combustion, reduced
emissions, reduced contamination of panel, safe heating* 
* All the above effects are of course heavily dependent on the construction of the individual stove and its normal usage. We strongly recommend that you check whether ROBAX® Energy Plus delivers the results you are looking for before you opt for a standard model.
News, Trade Fairs & Events
25.
April
Trade fair Ceramics Expo, Cleveland, OH, USA, 25.04 - 27.04.2017
05.
April
Trade fair Ceramics 2017, Tokyo Big Sight (East Hall #4), Japan, 05.04 - 07.04.2017
SCHOTT uses Cookies on this Website to enhance the user experience and provide the best possible Service. By continuing to browse the Website, you consent to our use of Cookies.