Standard moulds

Round bent



Source: Focus

Maximum Size Tolerance
h panel height 800 mm h ≤ 500 mm
500 mm < h ≤ 600 mm
h > 600 mm
± 1.0 mm
± 1.5 mm
Determined after first sample
lA bow length 1,000 mm lA ≤ 500 mm
lA > 500 mm
± 1.5 mm
± 2.0 mm
R bending radius Minimum: 225 mm


1 x angular bent



Source: Rüegg Cheminée AG

Minimum Maximum Size Tolerance
h panel height 170 mm 600 mm h ≤ 500 mm ± 1.0 mm
± 1.5 mm
l1 long side 390 mm 860 mm l1 ± 2.0 mm
l2 short side 60 mm 500 mm l2 ± 2,0 mm
α bending angle 90° 160° α See slot gauge


2 x angular bent



Source: Rüegg Cheminée AG

Minimum Maximum Size Tolerance
h panel height 170 mm 650 mm h ≤ 500 mm
500 mm < h ≤ 600 mm
± 1.0 mm
± 1.5 mm
l2 center section length 180 mm 630 mm l2 ± 1.0 mm
l1, l3 side section length 60 mm 310 mm l1, l3 ± 2.0 mm
α bending angle 90° 160° α See slot gauge


2 x angular bent – special mould 2 x 90°



Source: Rüegg Cheminée AG

Standard dimensions
Bending angle
Length of blade
Length of stretched glass
Height
Thickness of glass
90°
≤ 300 mm
< 1255 mm
200 mm - 650 mm
4 mm
Further dimensions on request.


Contact

Home Tech
SCHOTT AG

Hattenbergstrasse 10
55122 Mainz
Germany
 +49 (0)6131/66-3798
 +49 (0)3641/2888-9162
E-mail
Directions
More contacts
Top news
More news
Trade Fairs & Events

22.02 - 26.02.2012

Progetto Fuoco

Verona

20.02 - 23.02.2012

Intern. Armoured Vehicles

London

01.03 - 03.03.2012

Hearth, Patio, Barbeque Expo

Salt Lake City

More trade fairs