SCHOTT Home

Miracles become reality through ROBAX® Magic


Due to their thermal, physical and chemical material properties, ROBAX® Magic glass ceramic panels are intended for use as a resistant exterior cover for stoves and fireplaces.

The additional reflections of the flame backlash, minor soiling and the easy cleaning of the glass ceramic panels make ROBAX® Magic a genuine alternative to the conventional materials used for the interior lining of combustion space.

Thermal roperties
Dimensions & design
Material colours

Thermal properties

Temperature/time load


Temperature/time resistance

The temperature/time resistance establishes the minimum specifications for permissible temperatures for pre-defined stress times, below which no thermally induced tension cracking occurs.

The temperature/time resistance for even temperature distribution over the entire glass ceramic panel is shown in the following table.

Material characteristics for ROBAX® Magic panels if heated homogeneously:

Stress temperature Thom Stress time
700° C
750° C
775° C
800° C
825° C
> 6000 h
> 750 h
> 275 h
> 100 h
> 35 h


Remark:
When ROBAX® Magic is used, inhomogeneous temperature conditions on the panels appear. Due to the manifold influence factors it is impossible to provide a precise estimation of the temperature stress which occurs.

Coefficient of mean linear expansion
α (20, 700 °C) < 1,0 x 10-6 / K

Specific heat capacity
cp (20, 100 °C) ca. 0,8 x 103 J / (kg ·K)

Heat conductivity
λ (90 °C) ca. 1,6 W / (m·K)

Resistance to temperature gradients (RTG)
Resistance of the panel against internal temperature differences. No cracking due to thermal stress at temperature differences T ≤ 650 °C

Resistance to thermal shock (RTS)
Resistance of the panel against thermal shocks, if for example the hot panel is quenched with scavenging air or by mechanical contact. No cracking due to thermal stress at temperature differences T ≤ 650 °C

Dimensions & design

ROBAX® Magic is only available as customized cut-to-size panel.

Glass thickness
Design
Minimum dimension
Maximum dimensions (cuttings*)
4 mm
flat, drilling possible
100 x 100 mm
1,180 x 590 mm
This data is subject to change within the course of the product's further development.

Additional dimensions available upon request.


Material colours

ROBAX® Magic Black
ROBAX® Magic Grey
ROBAX® Magic White
black
dark grey
white
The surface opposite to the inner combustion chamber is knobbed.


Contact

Home Tech
SCHOTT AG

Hattenbergstrasse 10
55122 Mainz
Germany
 +49 (0)6131/66-3798
 +49 (0)3641/2888-9162
E-mail
Directions
More contacts
Top news
More news
Trade Fairs & Events

22.02 - 26.02.2012

Progetto Fuoco

Verona

20.02 - 23.02.2012

Intern. Armoured Vehicles

London

01.03 - 03.03.2012

Hearth, Patio, Barbeque Expo

Salt Lake City

More trade fairs