Due to their thermal, physical, and chemical material properties, ROBAX® Ambience glass ceramic panels are intended for use as a resistant and attractive exterior cover for stoves and fireplaces. ROBAX® Ambience can be decorated with a large choice of colors.


Thermal properties
Dimensions and Design
Material colors

Thermal characteristics

Temperature/time resistance
Up to temperatures of 500 °C, ROBAX® Ambience ensures that no temperature induced cracking due to thermal stress occurs.

α (20, 700 °C) < 1,0 x 10-6 / K

Resistance to temperature gradients (RTG)
Resistance of the panel against internal temperature differences. No cracking due to thermal stress at T ≤ 500 °C

Resistance to thermal shock (TSR)
Resistance of the panel against thermal shocks, if for example the hot panel is quenched with scavenging air or by mechanical contact. No cracking due to thermal stress at T ≤ 500 °C

Dimensions and design

ROBAX® Ambience is only available as customized cut-to-size panel.

Glass thickness
Design
Minimum dimensions
Maximum dimensions
4 mm
flat, drilling possible
100 x 100 mm
1,180 x 590 mm
Colour patterns
(using silk-screen printing)
up to 5 decoration colours per material colour available
This data is subject to change within the course of the product's further development.

Additional dimensions available on request.


Material colours

ROBAX® Magic Black
ROBAX® Magic Grey
ROBAX® Magic White
black
dark grey
white
The surface opposite to the inner combustion chamber is knobbed.


Contact

Home Tech
SCHOTT AG

Hattenbergstrasse 10
55122 Mainz
Germany
 +49 (0)6131/66-3798
 +49 (0)3641/2888-9162
E-mail
Directions
More contacts
Top news
More news
Trade Fairs & Events

22.02 - 26.02.2012

Progetto Fuoco

Verona

20.02 - 23.02.2012

Intern. Armoured Vehicles

London

01.03 - 03.03.2012

Hearth, Patio, Barbeque Expo

Salt Lake City

More trade fairs