SCHOTT Home

Mechanical properties

Density
ρ approx. 2,6 g/cm3 (bei 25 °C)

Bending Strength
σbB approx. 35 MPa

Impact Strength

The strength of glass ceramic is material constant. It is dependent on the size and thickness of the panel, the finish condition (edge working, drillings, etc.), usage conditions, (kind and distribution of defects on the surface), and the time related and kind of impact load and the type of panel installation. The norms to be fulfilled regarding the required strength resistance in the application field of fireplaces differ according to the individual region.