Excellent Heat Resistance
|
Excellent resistance to thermal gradients as well as shocks and the ability to resist very high temperatures up to 950 °C due to its nearly zero thermal expansion makes RESISTAN® as the prime choice for applications exposed to extreme operating conditions.
|
|
|
Thermal Data |
| Specific Heat Capacity cp (20-100°C) |
[J/(g·K)] |
0.80 - 0.85 |
| Thermal Conductivity λ(90°C) |
[W/(m·K)] |
1.6 - 1.7 |
| Max. Temp. Gradient (MTG) |
[K] |
400 - 800 |
| Thermal Shock (TSR) |
[°C] |
700 - 820 |
|
Temperature Time Load Capacity |
| Short Heating (1h) - [°C] |
Homogenous |
910 - 950 |
| Inhomogenous |
700 - 850 |
| Continuous Heating (5000h) - [°C] |
Homogenous |
450 - 750 |
| Inhomogenous |
400 - 660 |
|
Coefficient of Mean Linear Thermal Expansion (CTE) |
| α (-50 – 100°C) |
-0.8 - 0.6 x 10-6 K-1 |
| α (0 – 50°C) |
-0.8 - 0.6 x 10-6 K-1 |
| α (20 – 300°C) |
-0.4 - 0.9 x 10-6 K-1 |
| α (300 – 700°C) |
0.1 - 1.4 x 10-6 K-1 |
|
Please find additional information and definitions in our glossary.
|
All technical data are intended to serve as typical averages and are subject to change.
Detailed information on the different material types are documented in separate data sheets [more] or can be provided upon request. [more]
|
|