SCHOTT Home
Manifold Optical Properties


The RESISTAN® material family has a high transmittance for wavelengths covering the visible and infrared range. RESISTAN® can thus be used anywhere a high thermal resistance is needed in combination with excellent transparency.

Click on the respective wavelength range (UV, visible, IR) for detailed transmission graphs:
Transmission data were measured for RESISTAN® panels with a 4 mm thickness.
The infrared spectral range is subdivided according to DIN 5031, part 7[more]

Download RESISTAN® transmission graphs as Adobe Acrobat Reader (PDF) document:

schott_ag__resistan_transmission.pdf RESISTAN® Transmission Graphs
Optical Data
Abbé Number ne 546.1 nm 55.64
Abbé Number nd 587.6 nm 55.89
Refractive Index ne 546.1 nm 1.5468
Refractive Index nd 587.6 nm 1.5445
All Values were determined for clear transparent RESISTAN® 724-3.


Please find additional information and definitions in our glossary.

Data regarding the UV range and infrared range as well as detailed information about the different material types are documented in separate data sheets [more] or can be provided upon request. [more]



Contact

SCHOTT AG

Hattenbergstrasse 10
55122 Mainz
Germany
 +49 (0)6131/66-0
 +49 (0)6131/66-2000
E-mail
More contacts