Good mechanical strength of Resistan


Mechanical Data
Density ρ [g/cm³] 2.5 - 2.6
Modulus of Elasticity E ASTM C-1259 [10³ MPa] 84 - 95
Poisson's Ratio μ ASTM C-1259 0.25 - 0.26
Knoop Hardness HK0.1 / 20 ISO 9385 HK 0.1 / 20 570 - 680
Bending Strength σbB DIN EN 1288, Part 5, R45 [MPa] 100 - 160
Porosity ISO 9385 [%] 0
Roughness
(e.g. RESISTAN® 724-3, t = 4 mm)
[μm] Ra ≤ 0.20
Rms ≤ 0.25


Please find additional information and definitions in our glossary.

All technical data are intended to serve as typical averages and are subject to change.
Detailed information on the different material types are documented in separate data sheets [more] or can be provided upon request. [more]

Contact

SCHOTT AG

Hattenbergstrasse 10
55122 Mainz
Germany
 +49 (0)6131/66-0
 +49 (0)6131/66-2000
E-mail
More contacts