Outstanding Electrical Characteristics
|
Due to its low alkali content, RESISTAN® has very outstanding insulating properties. It is the ideal material for applications requiring an excellent insulator at high temperatures. |
|
|
Electrical Data |
| Specific Electrical Volume Resistance log ρ (250°C) |
[Ω·cm] |
6.6 - 7.0 |
| Specific Electrical Volume Resistance log ρ (350°C) |
5.2 - 5.6 |
| tk100 |
[°C] |
173 - 198 |
| Dielectric Constant εr (1 MHz, 25°C) |
|
6.3 - 7.8 |
| Dielectric Loss Tangent tan δ (1 MHz, 25°C) |
|
0.004 - 0.02 |
|
Please find additional information and definitions in our glossary.
|
All technical data are intended to serve as typical averages and are subject to change.
Detailed information on the different material types are documented in separate data sheets [more] or can be provided upon request. [more]
|
|