High Strength Against Chemical Attack
|
RESISTAN® is resistant to chemical surface attack and characterized by gas impermeability. Its smooth surface is free of pores and water-repellent.
|
|
|
The individual RESISTAN® materials are classified into the following chemical resistance classes. Translucent RESISTAN® 701-6 and opaque RESISTAN® 724-8 are extraordinary resistant in all categories (class 1).
|
Chemical Data |
| Acid Resistance Class S |
DIN 12116 |
1 - 3 |
| Alkaline Resistance Class A |
ISO 695 |
1 - 2 |
| Hydrolytic Resistance Class HGB |
ISO 719 |
1 |
|
Please find additional information and definitions in our glossary.
|
All technical data are intended to serve as typical averages and are subject to change.
Detailed information on the different material types are documented in separate data sheets [more] or can be provided upon request. [more]
|
|
Contact
SCHOTT AG
Hattenbergstrasse 10 55122 Mainz Germany
| +49 (0)6131/66-0 |
| +49 (0)6131/66-2000 |
E-mail
More contacts
|