Standard forms of delivery

The current status of availability by material and form of delivery has to be requested by the customer. Not all combinations are producible. Other forms of delivery are available on request.


General appearance

Transparent, translucent white, translucent bluegrey, opaque white, opaque grey, tinted.
One-sided nubs are available on request.

The surface texture depends on the thickness.
Polishing process provides “window glass” appearance.
Decoration is available on request.
Overview of dimensions: Cut-to-size panels
  Standard length Standard width Profile
Thickness   Min. - Max. Min. - Max.  
2 mm 50 – 1,555 mm 50 – 860 mm On request  
3 mm 50 – 1,930 mm 50 – 1,075 mm C, U, V
4 mm 50 – 1,930 mm 50 – 1,075 mm C, U, V
5 mm 50 – 1,930 mm 50 – 1,075 mm C, U, V
6 mm 50 – 1,930 mm 50 – 1,060 mm C, U, V
≥ 8 mm 50 – on request 50 – 960 mm C, U, V

Forms of delivery
Grinding profiles
SCHOTT NEXTREMA® glass-ceramic grinding profiles
Dimensional tolerances and material defects

With regard to the specific format all of the following characteristics refer to the net-size, as agreed upon with the customer. Other forms of delivery are available on request.


Dimensional tolerances of flat cut-to-size panels

Characteristics / Areas / Location
 

Tolerance  
Thickness t  
t = 2.0 mm
t = 3.0 / 4.0 / 5.0 mm
t = 6.0 mm
 
± 0.3 mm
± 0.2 mm
± 0.3 mm
Edge length l  
l ≤ 500 mm    
l > 500 mm    
± 1.0 mm
± 1.5 mm

 
Squareness (ISO 1101) (depending to the edge length l)  
l ≤ 500 mm    
l > 500 mm    
≤ 1.0 mm
≤ 1.5 mm

 
Flatness along the diagonal D (depending on edge length l)    
on request
 
 
Corner radius r  
r ≤ 5 mm    
r ≤ 20 mm    
r > 20 mm    
± 0.5 mm
± 1.0 mm
± 2.0 mm

 
Drilled holes  
Diameter of drilled holes
Borehole position to reference
 
± 0.5 mm
± 1.5 mm

Dimensional tolerances
Further data and information available on request.
News, Trade Fairs & Events
02.
March
Trade fair HPBExpo, Atlanta, USA, 02.03 - 04.03.2017
16.
January
Trade fair BAU 2017, Munich, Germany, 16.01 - 21.01.2017
SCHOTT uses Cookies on this Website to enhance the user experience and provide the best possible Service. By continuing to browse the Website, you consent to our use of Cookies.