Mechanical properties (at room temperature)

High intrinsic mechanical strength even under high temperatures

NEXTREMA® shows attractive mechanical strength without the need for additional toughening processes. Even under high temperatures NEXTREMA® shows exceptional mechanical stability, making it the material of choice where high mechanical strength and temperature resistance are needed.


Key properties
      Benefits
   
Bending strength of up to 168 MPa (for 4 mm thick material)
  • High mechanical strength without special toughening process, even at elevated temperatures
Knoop hardness of up to 625
  • Good abrasion resistance
Material density of 2,5 – 2,6 g/cm³
  • Lightweight material compared to ceramic or metal materials

ρ approx. 2.5 – 2.6 g/cm3
 

Density

E approx. 84 – 95 x 10³ Mpa
 

Modulus of elasticity
(ASTM C-1259)
 

μ approx. 0.25 – 0.26
 

Poisson‘s ratio
(ASTM C-1259)
 

HK0.1 / 20 approx. 570 – 680                
 

Knoop hardness
(ISO 9385)
 

σbB approx. 100 – 160 Mpa

Bending strength
(DIN EN 1288, Part 5, R45)  
 

Impact resistance      The impact resistance of NEXTREMA® depends on the kind of installation, size,
thickness and geometry of the panel, type of impact and especially on drilled
holes and their position in the material.

Therefore, information regarding impact resistance can only be given with
knowledge of the respective and defined application (especially in combination
with the technical standards regarding impact resistance that have to be met for
some applications). The quality of the grinding profile has an important influence
according to the impact resistance.


0 %
 

Porosity (ISO 9385)  

Material 724-3 (t = 4 mm)      Ra ≤ 0.20 μm
                                            Rms ≤ 0.25 μm    
 

Roughness
News, Trade Fairs & Events
25.
April
Trade fair Ceramics Expo, Cleveland, OH, USA, 25.04 - 27.04.2017
05.
April
Trade fair Ceramics 2017, Tokyo Big Sight (East Hall #4), Japan, 05.04 - 07.04.2017
SCHOTT uses Cookies on this Website to enhance the user experience and provide the best possible Service. By continuing to browse the Website, you consent to our use of Cookies.