Temperaturbegrenzer SEREB® SB Type X Series Data

Dimensions

Dimension (Unit:mm)
SEREB X
Structure
SEREB X Structure
1. Terminal
2. Base
3. Cover
4. Arm
5. Bond
6. Contact
7. PTC Ceramic
8. Bimetal Element

Ratings

Part
Number
Operating
Temperature
Internal
Resistance
Contact
Rating
Maximum
Holding
Voltage
Maximum
Breaking
Voltage
Minimum
Holding
Voltage
Maximum
Current in
Holding
SB72X2 72±5℃ ≦8mΩ DC10V/12A
6000 Cycle
DC5V/40A
100 Cycle
DC28V/5A
100 Cycle
2V
(25℃)
150mA
(25℃)
SB77X2 77±5℃
SB82X2 82±5℃
SB85X2 85±5℃

Safety Standards

Part Number UL TÜV
Made in Thailand Made in Thailand
SB72X2 E344840 R50251001
SB77X2
SB82X2
SB85X2

Messen & Events
30.
Mai
Messe Materials, Veldhoven, Niederlande, 30.05 - 31.05.2018
26.
Juni
Messe World Nuclear Exhibition, Paris, Frankreich, 26.06 - 28.06.2018
05.
September
Messe CIOE - China International Optoelectronic Expo, Shenzhen, China, 05.09 - 08.09.2018
17.
September
Messe Gastech, Barcelona, Spanien, 17.09 - 20.09.2018
Kontakt
SCHOTT AG
Christoph-Dorner-Strasse 29
84028 Landshut
Deutschland
E-Mail an SCHOTT+49 (0)871/826-0
SCHOTT verwendet auf dieser Website Cookies, um die Seiten optimiert darzustellen und das Nutzererlebnis zu verbessern. Durch die Nutzung unserer Seiten erklären Sie sich damit einverstanden.