10.04.2014, SCHOTT AG

SCHOTT’s glass laminates offer proven simultaneous protection against fire, burglary and ballistic threats

PYRANOVA® secure panels on display at Counter Terror Expo
Photo shows a pane of PYRANOVA® secure that was first subjected to a fire test for 30 minutes then attacked with a 9 mm Luger army pistol. The extremely hot glass laminate from SCHOTT resists three shots fired from a 9 mm caliber gun at a speed of 400 m/s. Photo: SCHOTT:
Photo shows a pane of PYRANOVA® secure that was first subjected to a fire test for 30 minutes then attacked with a 9 mm Luger army pistol. The extremely hot glass laminate from SCHOTT resists three shots fired from a 9 mm caliber gun at a speed of 400 m/s. Photo: SCHOTT:
Stafford (UK) & Jena (Germany), April 10, 2014 – The international technology group SCHOTT introduces the world's first specialty glass products to successfully withstand consecutive fire and ballistic attacks. SCHOTT is to exhibit five glass panels of its PYRANOVA® secure laminates, showing varying degrees of attack, including bullet and fire separately and simultaneously, at the upcoming Counter Terror Expo, 29th – 30th April at Olympia, London (booth M30).



The threat of wilful attack from both external forces and fire can be very real for a number of organisations, and therefore safeguarding employees, visitors and building contents of embassies, consulates and government buildings is paramount. “SCHOTT is leading the way in providing a glass laminate that can not only stop penetration by bullet, but then go on to also protect from fire directly afterwards or vice versa,” explains Martin Brown, Sales Manager for SCHOTT UK.

To meet these unique demands, SCHOTT developed the highly effective, yet compact, multifunctional laminates. This type of complex structure is necessary in order to ensure that SCHOTT’s new products are able to resist multiple simultaneous attacks, while offering a high level of transparency and thermal resistance.

To prove the effectiveness of its products, SCHOTT will display a series of five PYRANOVA® secure laminates. The 34 mm thick samples will be 1500 mm x 300 mm, weighing 78.5 kg/m². The glass laminates are bullet resistant according to EN1063: BR2NS and, even after having been shot at, can still fulfil the fire resistance category EI30. Both during and after a Molotov cocktail attack, SCHOTT's product is bullet resistant. Five scenarios are shown: original, shot at, burnt, shot at and burnt, burnt and shot at: “These demonstration laminates prove that the performance of our material fulfils several multi attack criteria and enables visitors to see the results close up,” says Martin Brown.

Background information:

PYRANOVA® secure has been subjected to a fire test and bullet attack immediately after one another. This type of trial involving a barrage of potentially destructive assaults was performed for the first time anywhere in the world. The tests were carried out in September 2013. The results were monitored and confirmed by two independent institutes, the Beschussamt Ulm (Ballistic test facility in Ulm) and the Institute for Building Materials, Solid Construction and Fire Protection (IBMB) at the Technical University of Braunschweig. The glasses met both of the test standards DIN EN 1364-1 (Fire Protection) and DIN EN 1063 (Bullet Resistance). Due to the fact that the European legislator only requires that protective glasses meet EN safety standards individually, SCHOTT became the world's first company to voluntarily subject its safety laminates to a combination of tests.

The development of the new safety glass range has received support from the Thuringian State Government and the European Regional Development Fund EFRE as part of the research project “2nd Generation Multifunctional Safety Glazing” (2011 FE 0156) since October 2011.

For more information, visit: http://www.schott.com/pyran/

PYRANOVA® is a registered trademark of SCHOTT AG.

Download link: http://www.schott-pictures.net/presskit/233188.cte2014 /

SCHOTT is an international technology group with 130 years of experience in the areas of specialty glasses and materials and advanced technologies. SCHOTT ranks number one in the world with many of its products. Its core markets are the household appliance, pharmaceutical, electronics, optics and transportation industries. The company is strongly committed to contributing to its customers’ success and making SCHOTT an important part of people’s lives with high-quality products and intelligent solutions. SCHOTT is committed to managing its business in a sustainable manner and supporting its employees, society and the environment. The SCHOTT Group maintains close proximity to its customers with manufacturing and sales units in 35 countries. Its workforce of 15,400 employees generated worldwide sales of 1.84 billion euros for the 2012/2013 fiscal year. SCHOTT AG, with its headquarters in Mainz (Germany) is owned by the Carl Zeiss Foundation.
SCHOTT is leading the way in providing a glass laminate that can not only stop penetration by bullet, but then go on to also protect from fire directly afterwards or vice versa. Photo: SCHOTT.
SCHOTT is leading the way in providing a glass laminate that can not only stop penetration by bullet, but then go on to also protect from fire directly afterwards or vice versa. Photo: SCHOTT.
Press contact
SCHOTT AG
Michael Müller
Hattenbergstraße 10
55122 Mainz
Deutschland
Phone: +49 6131/66-4088
Fax: +49 3641/2888-9180
Further information
SCHOTT AG
Salvatore Ruggiero
Vice President Marketing and Communication
Hattenbergstraße 10
55122 Mainz
Germany
Phone: +49 6131/66-4140
Fax: +49 3641/2888-9180
SCHOTT uses Cookies on this Website to enhance the user experience and provide the best possible Service. By continuing to browse the Website, you consent to our use of Cookies.