SCHOTT Glass and Glass-Ceramic Sealants for Technical Ceramics in High-Temperature Applications - New Datasheet now available!

SCHOTT has developed special glasses and glass-ceramics for the sealing of technical ceramics. These sealants, chemically resistant and stable at elevated temperatures can contribute to the stability of the ceramic applications over an extended period of time. For more information about SCHOTT´s Glass and Glass Ceramic Sealants, please refer to the new Datasheet “Glass and Glass-Ceramic Sealants for Technical Ceramics in High-Temperature Applications “available on our download page. Alternatively, you could also contact us directly at any of our competence centres near you.