15.06.2009, Advanced Optics
SCHOTT AG
Large Format Synthetic Fused Silica

Homogeneous and free from inclusions: SCHOTT “Lithosil” for lenses of up to 700 mm in diameter

Jena/Munich (Germany), June 15, 2009 — At “Laser – World of Photonics”, SCHOTT will be presenting a large plate made of the synthetic fused silica “Lithosil” in a typical format of 1050 x 580 x 35 mm. This exhibit stands for the expertise that SCHOTT has in manufacturing homogeneous, ultrapure and bubble-free blanks for large format lenses.

These products are now available on a standard basis in dimensions of up to 700 mm in diameter and 110 kg respectively. Furthermore, homogeneity of up to < 5 ppm is achieved and they are completely free of all types of inclusions or bubbles. These products are known for their extremely high transmission in the UV and VIS range, as well as extremely low stress birefringence.

The sample on display that is made of the synthetic fused silica “Lithosil” rounds off the portfolio of large format blanks that SCHOTT offers. At the same time, formats of up to 1000 mm in diameter can also be achieved using traditional optical glass types, such as N-BK7, LLF1 and others. Typical applications for large “Lithosil” blanks include astronomy and lithography, but also large format lenses for use in conventional optics.

“With these large formats, our unique expertise lies in customer-specific forming of shapes,” notes Peter Maushake, Product Manager at SCHOTT Advanced Optics for the “Lithotec” products. In addition to the dimensions presented here, a wide variety of different geometries are possible thanks to customer-specific slumping. “Our colleagues who work in sales and research and development support our customers in realizing their projects. Virtually anything is possible,” Maushake points out.

SCHOTT is an international technology group that sees its core purpose as the lasting improvement of living and working conditions. To this end, the company has been developing special materials, components and systems for 125 years. The main areas of focus are the household appliances industry, pharmaceuticals, solar energy, electronics, optics and the automotive industry. The SCHOTT Group is present in close proximity to its customers with production and sales companies in all its major markets. The Group’s approximately 17,300 employees generated worldwide sales of approximately 2.2 billion Euros in the fiscal year 2007/2008. The company's technological and economic expertise is closely linked with its social and ecological responsibility. The SCHOTT AG is an affiliate of the Carl-Zeiss-Stiftung (Foundation).

Number of characters: 1775 (including empty spaces)

Advanced Optics
SCHOTT AG
 
Further information:
Advanced Optics
SCHOTT AG
Christine Fuhr
PR Manager
Corporate Public Relations
Tel. +49 (0) 6131 / 66-4550
Fax +49 (0) 6131 / 66-4041
E-mail
 
back
 
 
Press

Press Releases

Every SCHOTT press release archived chronologically. More
Publications

Publications

Company portrait, customer magazine, annual report and information on our history, all available for download. More
Solutions magazine

Customer Magazine "SCHOTT solutions"

In both German and English, the magazine lands on your table or appears on your monitor: Articles, reports and interviews on ideas and solutions from SCHOTT to the technological challenges worldwide. More
Trade Fairs

Trade Shows & Events

SCHOTT exhibits its products at the most important trade shows around the world. All trade show and event dates at a glance. More
Image Database

Image Database

Images from the SCHOTT press archive for viewing and downloading. More
Media Contacts

Media Contacts

Find your contacts from our Public Relations department. More
Contact

SCHOTT AG

Hattenbergstrasse 10
55122 Mainz
Germany
 +49 (0)6131/66-0
 +49 (0)6131/66-2000
E-mail
More contacts
Trade Fairs & Events

24.11 - 27.11.2009

Pharmtech

Moscow

29.11 - 04.12.2009

RSNA

Chicago

01.12 - 03.12.2009

CPHI

Mumbai

02.12 - 04.12.2009

Semicon Japan

Tokyo

More trade fairs