SCHOTT Home

Optical Properties

Zumtobel Staff
Photo: Zumtobel Staff
BOROFLOAT® 33 is a clear and transparent colorless glass. The excellent transparency of BOROFLOAT® 33 both in the ultraviolet and also in the visible and near infrared range of light makes it ideal as a cover panel for many types of floodlights, high-power spotlights and sunbeds (up to operating temperatures of 450 °C). Its extra low inherent fluorescence (light emission), combined with very good surface quality, flatness and homogeneity, opens up a wide-range of possible applications for BOROFLOAT® 33 in optics, opto-electronics, photonics and analytical equipment.



Optical Properties of BOROFLOAT® 33 diagrams:

DispersionTransmissionTransmission in the UV-RangeTransmission in the UV-Range as a Function of TemperatureTransmission in the IR-RangeTransmission of BOROFLOAT® 33 in Comparison with Borosilicate Crown GlassReflection of BOROFLOAT® 33 in Comparison with BOROFLOAT® MReflection of BOROFLOAT® 33 in Comparison with BOROFLOAT® AR
Fluorescence Behavior of BOROFLOAT®33

Some materials have the ability to emit electromagnetic radiation after being activated by high frequency short-wave radiation of high energy intensity. This behavior is called fluorescence. It depends on the material’s purity and its structural characteristics as well as the energy per pulse, pulse rate and the excitation wavelength of the radiation.

BOROFLOAT® 33 is a highly transparent glass showing very weak fluorescence intensities in the visible light wavelength range.

Selected Standard Lasers and Related Wavelengths:

Wavelength
(nm)
Laser
Medium
Wavelength
(nm)
Laser
Medium
Wavelength
(nm)
Laser
Medium
308 XeCI 488 Ar 1047 Nd:YLF
325 HeCd 514.5 Ar 1053 Nd:YLF
337 N2 532 Nd:YAG 1064 Nd:YAG
350 XeF 632.8 HeNe 1153 HeNe
351.1 Ar 694.3 Ruby 1319 Nd:YAG
363.8 Ar 730-780 Alexandrite 1730 Er:YLF
427 N2 850 Er:YLF 2060 Ho:YLF
441.6 HeCd 905 GaAs 10640 CO2