Due to its low alkali content, BOROFLOAT® 33 acts as a high-power insulator. BOROFLOAT® 33 is, therefore, a suitable material for applications where good non-conductive properties at temperatures (up to 450 °C) are called for.

Because of the special structure of borosilicate glass BOROFLOAT® 33 has a neutron absorbing effect.

Dielectric Constants
(at 25 °C and 1 MHz)
εr 4,6
Loss Tangent
(at 25 °C and 1 MHz)
tan δ 37 x 10-4
Logarithm of the Electric Volume
Resistivity
lg ρ                    250 ºC
                         350 ºC
8.0 Ω x cm
6.5 Ω x cm


Electrical Properties of BOROFLOAT® 33 diagrams:

dielectric_constant.pdf Dielectric Constants
loss_tangent.pdf Loss Tangent
electric_volume.pdf Logarithm of the Electric Volume Resistivity
dielectric_breakdown.pdf Dielectric Strength