BMW Welt, München
BMW Welt, München

PYRAN® S-AR

De un vistazo

Hechos clave

PYRAN® S-AR

PYRAN® S-AR performs several important functions all at the same time. It offers clear visibility due to low residual reflection and up to 2 hours of additional protection in case of fire. PYRAN® S-AR is a monolithic, thermally toughened borosilicate glass that is anti-reflective on both sides due to the fact that it is manufactured using a dip-coating process. The glass is coated with a hard, weather-resistant and multi-layered interference system. As a result, light reflection of 8% with an uncoated glass can be reduced to 1% using coated borosilicate glass.


  • Borosilicat-SG
  • Classification:
    E 30 till 120
  • Reflection: 1%

Datos técnicos

Product Fire
Rating
Thickness Weight Ug-Value g-Value Light
Transmission
Sound
Reduction
acc. EN 13501
[mm]
[kg/m2]
[W/m2K]
[%]
[%]
[dB]
PYRAN® S E(G) 30 - 60
5
11,4
5,8
90
92
30
E(G) 30 - 120
6
13,7
5,8
90
92
31
E(G) 30 - 120
8
18,2
5,8
90
92
32
E(G) 30 - 120
10
22,8
5,8
90
91
33
E(G) 30 - 120
12
27,4
5,8
90
91
34

Contacto

SCHOTT
Technical Glass Solutions GmbH

Otto-Schott-Strasse 13
07745 Jena
Germany

 +49 (0)3641/681-4666
 +49 (0)3641/28889-311

Lorem ipsum dolor sit amet, consetetur sadipscing elitr, sed diam nonumy eirmod tempor invidunt ut labore et dolore magna aliquyam erat, sed diam voluptua. At vero eos et accusam et justo duo dolores et ea rebum. Stet clita kasd gubergren, no sea takimata sanctus est Lorem ipsum dolor sit amet

PYRAN® S-AR

PYRAN® S-AR performs several important functions all at the same time. It offers clear visibility due to low residual reflection and up to 2 hours of additional protection in case of fire. PYRAN® S-AR is a monolithic, thermally toughened borosilicate glass that is anti-reflective on both sides due to the fact that it is manufactured using a dip-coating process. The glass is coated with a hard, weather-resistant and multi-layered interference system. As a result, light reflection of 8% with an uncoated glass can be reduced to 1% using coated borosilicate glass.


  • Borosilicat-SG
  • Classification:
    E 30 till 120
  • Reflection: 1%
Product Fire
Rating
Thickness Weight Ug-Value g-Value Light
Transmission
Sound
Reduction
acc. EN 13501
[mm]
[kg/m2]
[W/m2K]
[%]
[%]
[dB]
PYRAN® S E(G) 30 - 60
5
11,4
5,8
90
92
30
E(G) 30 - 120
6
13,7
5,8
90
92
31
E(G) 30 - 120
8
18,2
5,8
90
92
32
E(G) 30 - 120
10
22,8
5,8
90
91
33
E(G) 30 - 120
12
27,4
5,8
90
91
34

SCHOTT
Technical Glass Solutions GmbH

Otto-Schott-Strasse 13
07745 Jena
Germany

 +49 (0)3641/681-4666
 +49 (0)3641/28889-311