Customer motifs can be added using a screen printing process. Two different color systems are available:

ceramic colors, which are blended into the glass surface by a thermal toughening process; organic colors, which are solvent-based and can be used, for example, on chemically toughened glass.

Color shades are mixed according to customer requirements or based on the RAL or Pantone standards. Multicolor printing is also possible.