Clear view in the Car Parks thanks to SCHOTT AMIRAN® for façades

Abu Dhabi Financial Center Car Parks

Project

The architects for the Financial Center in Abu Dhabi desired a clear view through not only the office building but also the adjoining car parks.
The outfitting of the office complex with anti-reflective glass was intended to maintain consistency of the design and the optical impression of the entire façade.

To achieve this, high demands were placed on reflection and transmission. AMIRAN® insulating glass,  consisting of thermally toughened safety glass and laminated safety glass, was the chosen solution and forms the exceptional façade of the car parks.

Download our Project Report Light

Material

SCHOTT AMIRAN® is a one or both side anti-reflective coated glass for a clear view inside and out, both day and night. Its non-sensitive, high-tech coating reduces reflections to less than 1% and allows up to 98% of the light to pass through uninhibited.

AMIRAN® provides clear viewing even under extreme brightness differences both in front of and behind the pane.
Salons et événements
27.
June
Salon commercial Sicherheitsexpo, München, Allemagne, 27.06 - 28.06.2018
14.
January
Salon commercial BAU, Munich, Allemagne, 14.01 - 19.01.2019
Modifier
Sur ce site Web, SCHOTT utilise des cookies afin d'optimiser l'affichage des pages et améliorer le confort et l'expérience de l'utilisateur. En continuant à naviguer sur ce site, vous déclarez les accepter.