PYRANOVA® special glass fits in seamlessly with sophisticated architectural design. The butt joint system with PYRANOVA® special glass, for instance, joins the glass panes together in a frameless manner with the help of a special silicone seal. This allows for the creation of light, smooth sheets of glass that are virtually endless and offer a clear view at all times. PYRANOVA® special glass in the butt joint system also allows for constructions that contain corners.

Caractéristiques techniques

Product Fire
Rating
Thickness Weight Light
Transmission
Ug-Value Sound
Reduction
acc. EN 13501-2
[mm]
[kg/m2]
[%]
[W/m2K]
[dB]
Interior
PYRANOVA® EW E (W) 30
7
17
89
5,6
33
PYRANOVA® EW EI (F) 15 / EW 30
11
26
87
5,4
36
PYRANOVA® 30 EI (F) 30
15
35
86
5,1
38
PYRANOVA® 45 EI (F) 45
19
44
85
5
38
PYRANOVA® 60 EI (F) 60
23
55
87
4,8
41
PYRANOVA® 90 EI (F) 90
37
86
84
4,8
44
PYRANOVA® 120 EI (F) 120
52
106
74
2,5
42
Exterior
PYRANOVA® EW EI (F) 15 / EW 30
10
24
87
5,4
36
PYRANOVA® EW EI (F) 20 / EW 30
14
32
86
5,2
38
PYRANOVA® 30 EI (F) 30
19
44
83
5
38
PYRANOVA® 45 EI (F) 45 / EW 60
19
44
85
5
38
PYRANOVA® 60 EI (F) 60
27
61
86
4,7
41
PYRANOVA® 90 EI (F) 90
40
93
83
4,1
44
PYRANOVA® 120 EI (F) 120
54
116
74
2,5
44

Contact

SCHOTT France SAS

6 bis rue Fournier
92110 Clichy
France

 +33 (0)140 873924
 +33 (0)140 873988

PYRANOVA® SF

PYRANOVA® special glass fits in seamlessly with sophisticated architectural design. The butt joint system with PYRANOVA® special glass, for instance, joins the glass panes together in a frameless manner with the help of a special silicone seal. This allows for the creation of light, smooth sheets of glass that are virtually endless and offer a clear view at all times. PYRANOVA® special glass in the butt joint system also allows for constructions that contain corners.
Product Fire
Rating
Thickness Weight Light
Transmission
Ug-Value Sound
Reduction
acc. EN 13501-2
[mm]
[kg/m2]
[%]
[W/m2K]
[dB]
Interior
PYRANOVA® EW E (W) 30
7
17
89
5,6
33
PYRANOVA® EW EI (F) 15 / EW 30
11
26
87
5,4
36
PYRANOVA® 30 EI (F) 30
15
35
86
5,1
38
PYRANOVA® 45 EI (F) 45
19
44
85
5
38
PYRANOVA® 60 EI (F) 60
23
55
87
4,8
41
PYRANOVA® 90 EI (F) 90
37
86
84
4,8
44
PYRANOVA® 120 EI (F) 120
52
106
74
2,5
42
Exterior
PYRANOVA® EW EI (F) 15 / EW 30
10
24
87
5,4
36
PYRANOVA® EW EI (F) 20 / EW 30
14
32
86
5,2
38
PYRANOVA® 30 EI (F) 30
19
44
83
5
38
PYRANOVA® 45 EI (F) 45 / EW 60
19
44
85
5
38
PYRANOVA® 60 EI (F) 60
27
61
86
4,7
41
PYRANOVA® 90 EI (F) 90
40
93
83
4,1
44
PYRANOVA® 120 EI (F) 120
54
116
74
2,5
44

SCHOTT France SAS

6 bis rue Fournier
92110 Clichy
France

 +33 (0)140 873924
 +33 (0)140 873988